Nylon 6/12 Rod

Nylon 6/12 (PA612), Extruded

Absorbs about a third the water of nylon 6/6 - 0.15% in 24 hours against 0.45%, and 3.0% at saturation against 8.5%. The grade for close-tolerance parts in wet or humid service. You pay for it in heat deflection, hardness and wear, so it is not a bearing grade.

  • Description
  • Features
  • Reviews
  • Nylon 6/12 exists for one reason: it absorbs about a third the water of nylon 6/6. Measured on the same method by the same manufacturer, 24-hour absorption is 0.15% against 0.45% and saturation is 3.0% against 8.5%. Since moisture pickup and the dimensional growth that follows it are the usual reason a nylon part drifts out of tolerance, 6/12 is what you specify when the part has to hold its size in wet or humid service. Tensile strength is 10,000 psi at yield on a 300,000 psi modulus, flexural strength 14,000 psi on a 350,000 psi flexural modulus, compressive strength 11,500 psi at 10% strain and hardness Rockwell M70 (R114).

    It is machined into close-tolerance bushings, rollers, guides, electrical parts and conveyor and power-engineering components. Melting point is 422F and continuous service 185F, with a 690 V/mil dielectric strength for insulating work. Be clear that the moisture stability is paid for everywhere else: heat deflection at 264 psi is only 142F against roughly 200F for 6/6, hardness and modulus are the lowest of the unfilled nylons, and at a 0.31 coefficient of friction with a 190 x 10^-10 wear factor it is the poorest bearing material in the range. Buy it for dimensional stability, not for load or wear. Natural is the only colour.

Material PA (Nylon)
Shape Rod
Profile Round
Manufacturing Method Extruded
Unit of Measure Ft